Facultad de Enfermería y Fisioterapia Salus Infirmorum

Estudio del efecto de distintos tipos de nanocargas en el comportamiento mecánico y térmico de un cemento óseo = (Record no. 12328)

MARC details
000 -LEADER
fixed length control field 04024nas a22003377a 4500
003 - CONTROL NUMBER IDENTIFIER
control field OSt
005 - DATE AND TIME OF LATEST TRANSACTION
control field 20210420163017.0
006 - FIXED-LENGTH DATA ELEMENTS--ADDITIONAL MATERIAL CHARACTERISTICS
fixed length control field m|||||r|||| 00| 0
007 - PHYSICAL DESCRIPTION FIXED FIELD--GENERAL INFORMATION
fixed length control field ta
008 - FIXED-LENGTH DATA ELEMENTS--GENERAL INFORMATION
fixed length control field 171219t2013 sp ||||| |||| 00| 0 spa |
022 ## - INTERNATIONAL STANDARD SERIAL NUMBER
International Standard Serial Number 1888-6116
040 ## - CATALOGING SOURCE
Transcribing agency Salus Infirmorum
245 00 - TITLE STATEMENT
Title Estudio del efecto de distintos tipos de nanocargas en el comportamiento mecánico y térmico de un cemento óseo =
Remainder of title Study of the effect of different nanofillers on the thermal and mechanical behavior of a bone cement /
Statement of responsibility, etc. Paz Jiménez E, Abenojar Buendía J, Cledera Castro MM, Ballesteros Iglesias Y, Forriol F, del Real Romero JC
500 ## - GENERAL NOTE
General note Este artículo se encuentra disponible en su edición impresa.
504 ## - BIBLIOGRAPHY, ETC. NOTE
Bibliography, etc. note Bibliografía: p.180-181
520 3# - SUMMARY, ETC.
Summary, etc. Objetivo:Estudiar el efecto de la adición de diferentes nanocargas en la resistencia mecánica y en el proceso de curado de un cemento óseo. Material y método: Se preparó un cemento óseo de formulación similar a los cementos comerciales, al que se añadieron nanotubos de carbono (MWCNT), un modificador de la tenacidad basado en copolímeros en bloque (Nanostrength®). Para evaluar el efecto sobre el cemento base, se utilizaron diferentes cantidades de carga, en un rango de entre 0,1 y 1% p/p (MWCNT) y entre 1 y 10% p/p (Nanostrength®). Se efectuaron ensayos de flexión, compresión y fractura para determinar las propiedades mecánicas y las propiedades térmicas. Resultados: Encontramos una disminución en la temperatura máxima alcanzada durante el curado del cemento con la adición de los MWCNT, sin verse afectadas sus propiedades mecánicas. En el caso del Nanostrength®, los resultados obtenidos no presentaron mejoras significativas en sus propiedades mecánicas, fundamentalmente la tenacidad, pero si un ligero aumento en su temperatura de curado y una disminución en el tiempo de fijación. Conclusión: La adición de diferentes porcentajes de nanotubos de carbono a la formulación base de un cemento óseo mejora sus propiedades térmicas sin reducir las propiedades mecánicas. El Nanostrength®, por el contrario, no mejoró el comportamiento térmico ni mecánico del cemento óseo.
520 8# - SUMMARY, ETC.
Summary, etc. Objective: To study the effect of the addition of different nanofillers on the mechanical properties and in the curing process of the bone cement. Methods: A bone cement of similar formulation to commercial cements was prepared in the laboratory. Two nanofillers were used: carbon nanotubes (MWCNT) and a toughness modifier based on block copolymers (Nanostrength®). To evaluate the effect on the cement, weigth loadings ranging from 0,1 to 1 wt% (MWCNT) from 1 to 10 wt% (Nanostrength®) were used. Bending, compressive and fracture test were achieved to determine their mechanical properties. In addition, thermal properties were studied. Results: The results show a significant decrease in the maximum curing temperature of the cement with the addition of MWCNT, without being affected its mechanical properties. In the case of Nanostrength®, significant improvements were not found in their mechanical properties, mainly tenacity, but a slight increase in temperature and a decrease of curing time of fixation were observed. Conclusions: The addition of carbon nanotubes to the basic formulation of a bone cement enhances the thermal properties without a reduction of the mechanical properties. Nanostrength® does not seem to improve the thermal and mechanical behavior of the bone cement.
653 14 - INDEX TERM--UNCONTROLLED
Uncontrolled term cemento óseo
653 14 - INDEX TERM--UNCONTROLLED
Uncontrolled term necrosis térmica
653 14 - INDEX TERM--UNCONTROLLED
Uncontrolled term propiedades mecánicas
653 14 - INDEX TERM--UNCONTROLLED
Uncontrolled term tenacidad a la fractura
653 14 - INDEX TERM--UNCONTROLLED
Uncontrolled term nanotubos de carbono
653 14 - INDEX TERM--UNCONTROLLED
Uncontrolled term bone cement
653 14 - INDEX TERM--UNCONTROLLED
Uncontrolled term thermal necrosis
653 14 - INDEX TERM--UNCONTROLLED
Uncontrolled term fracture toughness
653 14 - INDEX TERM--UNCONTROLLED
Uncontrolled term mechanical properties
653 14 - INDEX TERM--UNCONTROLLED
Uncontrolled term carbon nanotubes
773 ## - HOST ITEM ENTRY
Related parts -- 2013, v. 24, n. 3, p. 175-181
Title Trauma
856 ## - ELECTRONIC LOCATION AND ACCESS
Uniform Resource Identifier <a href="http://www.mapfre.com/fundacion/html/revistas/trauma/v24n3/docs/Articulo8.pdf">http://www.mapfre.com/fundacion/html/revistas/trauma/v24n3/docs/Articulo8.pdf</a>
Link text Acceso al documento
942 ## - ADDED ENTRY ELEMENTS (KOHA)
Source of classification or shelving scheme Universal Decimal Classification
Koha item type Artículo de revista
Holdings
Withdrawn status Lost status Source of classification or shelving scheme Damaged status Not for loan Collection code Home library Current library Date acquired Total Checkouts Full call number Barcode Date last seen Price effective from Koha item type Public note
    Universal Decimal Classification     Non-fiction Revistas y artículos Revistas y artículos 25/11/2019   PP14 v24(3):175-181 25/11/2019 25/11/2019 Artículo de revista Cajonera

Powered by Koha